Your Current Location : Home > PRODUCTS > Kumho Korea
Charpy impact strengh:
Testing Conditions:3.2mm,23℃
Testing Standard:ASTM D256
Testing Result:14-18
Testing Unit:kg.cm/cm
Application:Plate material
Speciality:High gum power,wear resistant
Melt flow index:
Testing Conditions:220℃,10kg
Testing Standard:ASTM D1238
Testing Result:16-20
Testing Unit:g/10 min
Application:Plate material
Speciality:High gum power,wear resistant